I am currently running at 2.12 minutes TAL using Indium 8.9H...
- Apr 05, 2011
by
rem
It's all relative to your Zone Temps and the thermal profile...
- Apr 07, 2011
by
A Very Frazzled Man
My oven profile is 155,160,165,180,220,245,255,227 Cooling Z...
- Apr 07, 2011
by
rem
Clearly you are above liquidus for too long so you can eithe...
- Apr 07, 2011
by
Graham
Thanks Graham that's what I'm thinking. I'm gonna have to st...
- Apr 07, 2011
by
rem