Views: 3562
I hope to get some feedback here. I have a SMD connector tha...
- Jul 08, 2011
by
leadthree
Your images are depicting signs of voiding. Some voiding is ...
- Jul 08, 2011
by
A Very Frazzled Man
I see bare copper on top of some of the leads. Maybe that's...
- Jul 11, 2011
by
ScottE