Can a bare PCB be ESD-sensitive ? If yes , in what conditions ?

reply »

#65738

Is a bare PCB ESD-sensitive ? | 11 January, 2012

It depends. * A common bare PCB IS NOT ESD sensitive and is a static generator * A less uncommon PCB with embedded parts IS ESD sensitive and is a static generator