Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 7986
With a large number of you out there building rigid-flex boa...
- Jan 11, 2012
by
cobhambill
215 to 220 deg.C peak reflow. We bake then store all PCB's ...
- Jan 12, 2012
by
SWAG
How are the vias failing? Barrel crack?
...
- Jan 12, 2012
by
blnorman
Isola water pressure. Between a 210°C normal tin lead cycle ...
- Jan 12, 2012
by
davef
I would recommend that you turn toward your PCB supplier pro...
- Jan 13, 2012
by
aci
The via's are cracking which then is causing all kinds of pr...
- Jan 17, 2012
by
cobhambill
I am wondering if the failurs that people see are discovered...
- Jan 19, 2012
by
cobhambill