we are currently developing a 180 degs downhole tool and are... - Mar 21, 2012 by Torch
Downhole solder suggestions, in order of preference are: * ... - Mar 21, 2012 by davef
thanks for the info :) ... - Mar 21, 2012 by Torch
What solder alloy are you using at the moment which is comin... - Mar 21, 2012 by Graham
To have an Operating Temp (Tool Classification) within your ... - Mar 21, 2012 by JAX