Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 10228
We are thinking of switching over from sac305 to sn100. Has ... - Apr 16, 2012 by kkay
I'd say it depends on the whole process you have. With... - Apr 17, 2012 by gaz
Actually we were looking into it for our selective solder pr... - Apr 17, 2012 by kkay
We started with SN100C from the very beginning when we purch... - Apr 18, 2012 by dyoungquist
kkay: I'm not real clear on where in the assembly process fl... - Apr 20, 2012 by davef
Only at our selective solder process. ... - Apr 20, 2012 by kkay
We are using SN100C in both our wave and selective machines ... - Apr 21, 2012 by Ed Mentzer
SN100C is being used by 95% of our customers over the SAC305... - May 04, 2012 by Steve