I had send my coating board to the test lab for adhesion coa...
- May 09, 2012
by
Umar
It's good that you're consistent. Troubleshooting an inconsi...
- May 10, 2012
by
davef
Hi Dave,
Thanks on yoru prompt reply,
Can help to shar...
- May 17, 2012
by
Umar
We us a lot of 1B31 it could be one of the most common coati...
- May 18, 2012
by
KaHrpr
Umar
Chapter 7 of IPC-HDBK-830, Guidelines for Design, Se...
- May 18, 2012
by
davef
I'll chime in here as well. If you have adhesion problems, ...
- May 18, 2012
by
blnorman
I use Trace and certainly recommend them. I actually just ha...
- May 31, 2012
by
jdumont
I use Trace Labs and certainly recommend them.
I actuall...
- May 31, 2012
by
jdumont
Hi Norman...
Thansk on yoru input, actually my adhesion ...
- Jun 01, 2012
by
Umar
Neither the Omega meter nor the IC are officially "destructi...
- Jun 01, 2012
by
blnorman
Umar, it may never be solved. Some coatings just do not stic...
- Jun 08, 2012
by
Lou