Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 12895
We are currently using an ACE K.I.S.S. 104. We used SN100 so... - Jun 21, 2012 by grauen06
Check your nitrogen. It sound like you do not have any. ... - Jun 21, 2012 by KaHrpr
We are using Nitrogen from Dewer tanks. We have purchased a ... - Jun 22, 2012 by grauen06
Is this a new process or are you experiencing a change in re... - Jun 22, 2012 by Hegemon
I have had Selective issues such as yours on two very differ... - Jun 22, 2012 by Frank Garcia
It sounds like the flux is not holding up during the solderi... - Jun 29, 2012 by tommyg_fla
We have not tried baking the boards yet. We are first going ... - Jun 29, 2012 by grauen06
never heard about Seho powerselective?? ... - Jul 11, 2012 by seif
The Alpha EF-9301 flux worked great! We went from ~4 solder ... - Sep 14, 2012 by grauen06
Grauen06-Glad to hear it worked out for you. If you adjust y... - Sep 14, 2012 by Frank Garcia