Hello folks,
we would in certain cases run a PCB second t...
- Jan 31, 2013
by
Evtimov
Are you talking about double sided reflow or just multiple p...
- Jan 31, 2013
by
dontfeedphils
Let's say I have an open joint on a BGA and I want just to r...
- Jan 31, 2013
by
Evtimov
If you have a hard-gold on your pads, it's not a problem. Ha...
- Feb 01, 2013
by
ENIAC
Regardless of the surface finish, you should try to limit th...
- Feb 01, 2013
by
dyoungquist
Thank you guys. You keep adding valuable information here. I...
- Feb 01, 2013
by
Evtimov
In agreement with Evtimov. Max 5 reflow cycles.
Something l...
- Feb 01, 2013
by
Hegemon
From some previous article I read (sorry, don't have citatio...
- Feb 01, 2013
by
isd.jww
Thank you all for the input. There is another concern. Do yo...
- Feb 07, 2013
by
Evtimov
I would consider wave solder as a cycle, in that for the mos...
- Feb 07, 2013
by
Hegemon
Hegemon,
my thinking was pretty much the same. I will pro...
- Feb 08, 2013
by
Evtimov