A question for all you wave experts out there:
We run our...
- Feb 20, 2013
by
caurbach
We agree with all of what Patrick has said. Hopefully your e...
- Feb 21, 2013
by
Pete B
Pete,
It would even be better if the wave machine manufac...
- Feb 22, 2013
by
Patrick Bruneel
Our new Soltec Delta 3 has this feature (they call it mainwa...
- Feb 22, 2013
by
caurbach
Caurbach,
Higher preheat and longer dwelltime will fix yo...
- Feb 22, 2013
by
Patrick Bruneel