Has anyone experienced bridging on topside (solder destination side) surface mount devices after wave soldering? We x-rayed 100% of the placements after smt re-flow with no issues. When the same placements were x-rayed after the tht wave solder process, bridging was evident from thermal planes to leads on nearly every assembly. We have found that a "dollop" of peelable solder mask on the underside of the components provides enough insulation to minimize the issue. Should I work on the wave profile? Is the solder mask a good idea?