We aquired an ERSA ECOSELECT 2 selective soldering machine. ...
- Apr 25, 2013
by
Dback
Hi,
I was using different brand machine but it will behav...
- Apr 25, 2013
by
Evtimov
Evtimov, thanks for your reply.
Yesterday was our first d...
- Apr 25, 2013
by
Dback
Evtimov, thanks for your reply.
Yesterday was our first d...
- Apr 25, 2013
by
Dback
Do you watch when it is doing the wave height test?
Watch i...
- Apr 29, 2013
by
Stephen
We have a Versaflow 40/50 and ours is setup like this.
We...
- Apr 29, 2013
by
Bill Axler
Stephen, Bill,
Thaks for your input.
We are currently ...
- May 01, 2013
by
Dback
Kurtz had a guy that was great with the machine.
I strong...
- May 02, 2013
by
Stephen
Stephen,
We are now running with 99.999 N, New nozzles an...
- May 08, 2013
by
Dback
Guys, thank you for your advice about Adipic Acid, it's an a...
- May 16, 2013
by
ENIAC
OK guys, we got our Adipic acid. What is the preferred metho...
- Jun 06, 2013
by
azhiker
azhiker, for me I selected method A. But I don't turn off wa...
- Jun 06, 2013
by
ENIAC
I used method 'A' but I leave the wave on. I use a stainles...
- Jun 06, 2013
by
Bill Axler
Bill, ENIAC, Thank you for your input. I'll do some research...
- Jun 06, 2013
by
azhiker
Bill, ENIAC, Thank you for your input. I'll do some research...
- Jun 06, 2013
by
azhiker
i've a competitor selective soldering and i would like test ...
- Aug 28, 2013
by
herve-35
You do not need much. We just take out pencil style stainle...
- Aug 29, 2013
by
Bill Axler