we are using acrylic conformal coating on the PCB. Under the...
- May 08, 2013
by
Steven Chen
What happens when you rework those non-coated areas? Please ...
- May 08, 2013
by
davef
this is one of my project. I have tried to remove coating on...
- May 09, 2013
by
Steven Chen
First, it appears that your solder mask and your coating mat...
- May 09, 2013