Hi guys, Whats actually Delta T ? As i know,its applic... - May 18, 2013 by kumar
Delta T is the temperature difference between the lowest and... - May 20, 2013 by JAX
Hi there.... Appreciate your info on this.As mentioned,th... - May 20, 2013 by kumar
I don't get it... Who cares if the zones on your oven are... - May 20, 2013 by JAX
Well, you wouldn't want 100 deg difference from zone to zone... - May 20, 2013 by Hegemon
Thanks to everyone for your answers... Delta T represents... - May 20, 2013 by kumar
Delta-T in reflow generally means 2 things - difference in t... - May 21, 2013 by Hussman