Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2624
Hola;
I have some PCBs with more than 1 year in its origina...
- Jul 22, 2013
by
Jorge_Quijano
What is the pad surface finish on these boards? I know OSP ...
- Jul 22, 2013
by
dyoungquist
I have Ag & ENIG finishes, for Ag I've seen some oxidation, ...
- Jul 22, 2013
by
Jorge_Quijano