Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2259
We had a solder joint problem in gold plated PLCC68 ic. We ...
- Jul 26, 2013
by
anilw2006
If there is a way to pre-tin the parts, that might help in f...
- Jul 26, 2013
by
Evtimov
Thanks for support.
Is it any special process of pre-tinng?...
- Jul 29, 2013
by
anilw2006