Hola I have this connector (atached image) for Wave Solder ... - Jul 30, 2013 by Jorge_Quijano
How full is the barrel actually getting? Per IPC-A-610, 100... - Jul 30, 2013 by dyoungquist
It has about 50-60%, we do not have equipmet to get an accur... - Jul 30, 2013 by Jorge_Quijano
Did you try increasing the top side preheaters? ... - Jul 30, 2013 by DeanM
Not yet, my next run will be tomorrow, I will try, let's see... - Jul 30, 2013 by Jorge_Quijano