I'm looking for evidence to support, or disprove, the use of...
- Oct 08, 2013
by
A Very Frazzled Man
Here's something from Indium that I had saved...
...
- Oct 08, 2013
by
dontfeedphils
Thanks Phil!
...
- Oct 08, 2013
by
A Very Frazzled Man
I think the critical item is that you are soldering in a red...
- Oct 11, 2013
by
Hegemon
We do in fact see a reduction in soldering defects, most esp...
- Oct 14, 2013
by
Hegemon
Another benefit to low O2 levels with Pb Free is increased m...
- Oct 15, 2013
by
CAPSE
Your 3rd paragraph hits it on the head, Frazz. Especially w...
- Oct 16, 2013
by
Hegemon