Hello, We've just started using VIGON A200 in our Aqueous... - Nov 21, 2013 by Luciano
The last time I got corroded parts out of my wash was when m... - Nov 21, 2013 by robgd3
Thanks for the tip! The DI tanks are brand new. Water ... - Nov 21, 2013 by Luciano
Are you using zestron corrision inhibiter Ci20 also? ... - Nov 25, 2013 by processman
Hi! I haven't found any info about that product. I can't ... - Nov 26, 2013 by Luciano
Hi, Its a zestron product which we have used for many y... - Nov 26, 2013 by processman
Thanks! ... - Nov 27, 2013 by Luciano
Insure your rinses are only 25 to 30-seconds each. Also ther... - Dec 03, 2013 by cpitarys
Thanks for the advice! ... - Dec 06, 2013 by Luciano