Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3830
Our contract manufacturing agency have procured pcbs from a...
- Mar 18, 2014
by
saravanan
I can't picture much of what you're saying, not for nothing,...
- Mar 19, 2014
by
davef
Please refer the attached jpegs, The problem is noticed afte...
- Mar 25, 2014
by
saravanan
Have you tried to bake the boards before you process them?
...
- Mar 25, 2014
by
Evtimov
The boards are baked for 2 hours at 120 deg C
Regards,
...
- Mar 25, 2014
by
saravanan
The first impression I get is that the mask was applied over...
- Mar 25, 2014
by
SweetOldBob
It is Solder Mask on Bare copper, The land finish is HASL as...
- Mar 25, 2014
by
saravanan
Ok lets put it this way. If the PCB house used a high qualit...
- Mar 25, 2014
by
SweetOldBob