Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6758
We are in the process of launching a new product and found r... - Apr 04, 2014 by Gary M
237C max is on the low end for SAC305, especially if you hav... - Apr 05, 2014 by SweetOldBob
The middle picture shows what looks to be solder balls litte... - Apr 05, 2014 by davef
The 237*C is under the inductor with aTAL of 48s. I worked... - Apr 05, 2014 by Gary M
It's right there in front of you. Not enough overall temper... - Apr 07, 2014 by Hegemon
Gary, We are missing something here. I see no evidence of r... - Apr 07, 2014 by Sr. Tech
I drilled a small hole from the other side in order to get m... - Apr 07, 2014 by Gary M
Found the issue. The footprint is incorrect. The inductor ... - Apr 07, 2014 by Gary M
Ahhh...now this makes sense. Glad you found the issue. Ga... - Apr 08, 2014 by Sr. Tech