Is anyone running reflowing in a vacuum oven to achieve void... - Jun 11, 2014 by SteveO
I don't fully understand what you are trying to do... 1. ... - Jun 12, 2014 by JAX
I am looking into Vapor Phase with Vacuum and Inline Reflow ... - Jun 12, 2014 by SteveO
For Vapor Phase: approximately .04 bar or 30 torr for aroun... - Jun 12, 2014 by JAX
Thanks. That helps. ... - Jun 13, 2014 by SteveO