Hello,
I'm fighting with problems of random solder balls ...
- Nov 13, 2014
by
grimus
Hola,
I've used the free e-book that I'm attaching when ...
- Nov 13, 2014
by
Jorge_Quijano
Are you experiencing the solder balls on the opposite side o...
- Nov 14, 2014
by
tombstonesmt
Same side (component side) if You give me e-mail I can provi...
- Nov 15, 2014
by
grimus
Sounds like your snap off profile needs adjustment. More tha...
- Nov 17, 2014
by
tombstonesmt
Probably not all the overpinted paste is flowing onto the jo...
- Nov 19, 2014
by
Graham
Could be. I am making overprint to achieve proper amount of ...
- Nov 25, 2014
by
grimus