Hi We are using Universal carrier for a 2 sided PCB, whe... - Mar 02, 2015 by VB
I would presume you reflow the top of the board first. Use t... - Mar 03, 2015 by sarason
Hi I also forgot to mention, top side is reflowed first ... - Mar 03, 2015 by VB
A couple of things that have helped me with solder ball issu... - Mar 03, 2015 by robgd3