Hi guys can you tell me what oa stands for when talking...
- Jul 29, 2001
by
JOHNW
OA: as in Organic Activated type of Solder paste, meaning th...
- Jul 30, 2001
by
Welcome to SMTnet.
The previous poster is correct. For m...
- Jul 30, 2001
by
davef