Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
need help in finding the high temp. solder paste (> 221 deg... - Jan 26, 2000 by Tuan Bui
Tuan - How about Sn/0.7Cu? It's M.P. is 227 and it's r... - Jan 26, 2000 by
Tuan: Consider Sn 96.5/Ag 3.5 or Sn10/PB88/Ag02 also. As ... - Jan 26, 2000 by davef
I've tried Indium NC-SMQ92(96.5Sn 3.5Ag) on these MCMs and ... - Jan 27, 2000 by Tuan Bui
Tuan - One of the reasons I suggested pre-tinning (aside ... - Jan 27, 2000 by
We used Promosol Sn96.5/Ag 3.5 during our initial qualifica... - Jan 30, 2000 by Paulvannan
Glenn and Paul have hit the nail right on the head. Contin... - Apr 12, 2000 by
Tuan Bui