Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 9150
Hi all,
Am new to SMT here.
I have a very thin laminat...
- Jan 26, 2017
by
Joshua Goi
Consider that printing may not be the only approach to getti...
- Jan 27, 2017
by
davef
> Hi all,
>
> Am new to SMT here.
>
> I...
- Jan 30, 2017
by
Robl
so, why are your laminates warped? What needs to be done to ...
- Jan 30, 2017
by
davef
Thanks Rob.
I'm not so sure in a mass production environm...
- Jan 30, 2017
by
Joshua Goi
I just assume when you have laminates that thin, it will inv...
- Jan 30, 2017
by
Joshua Goi
Tacsil is another product you might try.
...
- Jan 30, 2017
by
SWAG
Looks like a similar product to magic resin.
Thanks I'll ...
- Jan 30, 2017
by
Joshua Goi
Hi Joshua,
We ran 150K per week this way, you just need ...
- Jan 31, 2017
by
Robl
Hi Rob,
So do you have to constantly remove the old adhes...
- Jan 31, 2017
by
Joshua Goi
Dispensing: You can dispense for 0201 and above
Warped la...
- Jan 31, 2017
by
davef
Hi Joshua,
No, the adhesive lasts 2 or 3 runs. The adhes...
- Feb 01, 2017
by
Robl
Thinking very well
...
- Jul 28, 2018
by
eblusmart