Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 7269
We're currently using no-clean flux (SR-12) in a no-clean ma... - Mar 20, 2017 by u4bga
No clean is giving us problem in ICT. Other than that, a coa... - Mar 21, 2017 by Evtimov
Hi...i have a question. After you solder a circuit board, wh... - Nov 02, 2017 by JardCrocker
For low volume hand assembly, deionized water or IPA should ... - Nov 02, 2017 by dwl
On the flux reside issue that is gumming up your test probe ... - Nov 03, 2017 by davef
On your question about reliability ... " Is there testing we... - Nov 03, 2017 by davef
regarding dwl comment, "For low volume hand assembly, deioni... - Nov 03, 2017 by davef
IPA and DI water are both very common and effective methods ... - Nov 03, 2017 by dwl
Hello guys, In our company we use CS-FLUX for reballing p... - Mar 05, 2019 by pcMax