Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
My company is just beginning in SMT. We are using a glue a... - Dec 21, 1999 by John Sims
We had the same concern and decided to use 0603 components ... - Dec 21, 1999 by
I have been soldering 0603 components on the bottom side us... - Dec 21, 1999 by
John, we have waved 0603 packages for a long time, We have... - Dec 21, 1999 by RDR
Hi John, I�ve seen problems some sites have or had with br... - Dec 22, 1999 by Wolfgang Busko
John Sims