Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 7663
I have a few LED pcb's that have an aluminum substrate that ... - Jun 23, 2017 by jchris
I haven't tried doing these, personally...but... - Try a ... - Jun 23, 2017 by robgd3
Here's a good IR preheater that you should look at: www.p... - Jun 24, 2017 by PACE-Worldwide
I have worked with a few of my customers to rework heavy LED... - Jul 07, 2017 by CAPSE
A picture shows more than a thousand words. If you show us t... - Jul 07, 2017 by Evtimov
We had very little success reworking these type of boards. W... - Jul 07, 2017 by tombstonesmt
Defective LED's that I need to replace. ... - Jul 07, 2017 by jchris
Sounds interesting CAPSE, but unwieldy. Thanks. ... - Jul 07, 2017 by jchris
Hi jchri, Evtimocv is correct. I think there is somebo... - Jul 07, 2017 by Heros Electronics
I agree ... I'll get a photo off on Monday when I get back t... - Jul 07, 2017 by jchris
Just a random thought, but we had an issue with having to re... - Jul 10, 2017 by PhilC
> I have a few LED pcb's that have an aluminum > sub... - Jul 12, 2017 by Bill Axler
Not much help for what you have manufactured but you could t... - Jul 12, 2017 by Russfrom NH
We are using hot-plate. It is the safest method to rework al... - Jul 13, 2017 by Jandon
Hello ALL Good day , it is Amalia from HX Circuit Technolog... - Aug 31, 2017 by Amalia Zeng
Thanks for all of your suggestions. I ended up borrowing a P... - Aug 31, 2017 by jchris