Hi,
I'm facing smear after printing on DEK288 using reverse...
- Dec 10, 1999
by
Tracy Guo
Tracy,
I would check the squeegee blade for wear at the e...
- Dec 10, 1999
by
Gary Kemp
Tracy,
Gary made some good points, you could also to check...
- Dec 15, 1999
by
Check the print gap and check the clamp edges,
sometimes th...
- Dec 16, 1999
by
Tracy Guo