Anyone who knows how to prevent such flaw?
Tombstones are...
- Aug 11, 2017
by
Heros Electronics
> Anyone who knows how to prevent such
> flaw?
>...
- Aug 13, 2017
by
Dawson
> There is no solution in above case, this is
> caus...
- Aug 14, 2017
by
Spoiltforchoice
Any of the comments so far could be valid. To add my opinion...
- Aug 14, 2017
by
DeanM
Here is some food for thought. Try to answer these questions...
- Aug 14, 2017
by
Evtimov
God I hate the formatting of my post!
...
- Aug 14, 2017
by
Evtimov
Not enough solderpaste. Uneven solderpaste volume on pads. B...
- Aug 16, 2017
by
DucHoang
I do not see anything obvious that would cause a therma...
- Aug 17, 2017
by
Sr. Tech
There is DFM Design for Manufacturing, but now I see DFF Des...
- Aug 17, 2017
by
SweetOldBob
The first reply from Tsvetan Usunov already answered your qu...
- Aug 18, 2017
by
Stivais
> The first reply from Tsvetan Usunov already
> answ...
- Aug 24, 2017
by
Heros Electronics