Hi all, a lifted lead (FP 0,5mm pitch) with a wire soldered to it needs proper protection against tear off. What kind of coating is appropriate, should be dispensable and fast drying.

Thanks in advance

Wolfgang

reply »

#8397

Re: patchproblem lifted lead | 30 November, 1999

Hello Wolfgang Try looking in the process guides section of Circuit Technologies web site. Their recomendation is to bond the jumper wire to the board within 6mm of the lead with hot melt glue, cyanoacrylic glue or adhesive dots. John Thorup

reply »

#8398

Re: patchproblem lifted lead | 30 November, 1999

Wolfgang: Made a mess of things now, eh??? Try:

Masterbond Product UV15-7TK1A Dymax 911

Ta

Dave F

reply »

Brian W.

#8399

Re: patchproblem lifted lead | 30 November, 1999

I have used Loctite, RTV3145, or Tak-Pak to secure the wire. As John said, the wire is usually secured to the board near the lifted lead, and usually at 1/4 inch intervals along the way.

Brian W.

reply »

#8400

Re: patchproblem lifted lead | 1 December, 1999

Hi Dave, yes messy, that�s the result of trying to use the newest chips available, getting the first shot (prototype chips) and building a couple of hundred boards and than detecting that the protos do not what they are supposed to do.As our market grows the problems grow. We got to deliver them anyway.