Hello, We are having difficulty soldering the above BGA. ... - Aug 21, 2018 by Hussman
Doesn't look like it would be deliberately high temp for it'... - Aug 22, 2018 by Robl
Hi rob, I did request info from Kingston but their on-lin... - Aug 22, 2018 by Hussman
Got the solder profile, but can't direct mail you as for som... - Aug 23, 2018 by Robl
If you can scrap a board and part then drill a small hole th... - Aug 23, 2018 by Stephen