Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6368
Is there anything to watch out for when purchasing older AOI... - Oct 06, 2018 by Reckless
Hello Reckless, My name is Brian D'Amico. I am the presi... - Oct 07, 2018 by bdamico
Thank you for responding. Is everything still linux based? ... - Oct 07, 2018 by Reckless
Hi Reckless, PM me and I'll send you the contact details fro... - Oct 08, 2018 by Robl
One of the reasons I am looking at older AOI inspection syst... - Oct 10, 2018 by Reckless
Hello Reckless, No all of our MIRTEC systems are Windows ... - Oct 10, 2018 by bdamico
We have 2 Mirtec AOI's in our plant and can say they are ver... - Oct 10, 2018 by Doug Christen
How much do they run? Older Marantz 22X systems are run... - Oct 11, 2018 by Reckless
I would suggest spending the extra money and getting the Mir... - Oct 11, 2018 by Doug Christen
Hello Doug, Thank you for the reference on our vintage MV... - Oct 11, 2018 by bdamico
We have a pair of old 22XDL's that are just used for heritag... - Oct 12, 2018 by Robl
Reckless, why would you get desktop machine? AOI machine ... - Oct 15, 2018 by Evtimov
Mostly because its outside the budget currently. We may look... - Oct 15, 2018 by Reckless
Be careful about used AOIs, some of the companies have truly... - Oct 15, 2018 by Comatose
That's incorrect. 3D aoi is extremely useful for determining... - Oct 17, 2018 by Doug Christen
What is slope? Solder flow issues seem unlikely for long run... - Oct 17, 2018 by Reckless
I have one of those collecting dust in storage (well, the tr... - Oct 17, 2018 by Comatose
I'll be interested depending on price. I don't have much of... - Oct 20, 2018 by Reckless
My pick and place machines are 10+ years old so I might be i... - Oct 20, 2018 by Reckless
THE AOI system is good for presence and polarity only ... - Oct 23, 2018 by tech1
Will it not work for soldering defects (solder bridges, shor... - Oct 23, 2018 by Reckless
It will in a limited fashion. It is a scanner and when using... - Oct 24, 2018 by tech1