Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi What is the possible cause of non-wetting of solder pas... - Oct 27, 1999 by
Chris: Typical non-wetting causes are: * Poorly controll... - Oct 28, 1999 by davef
Hi Dave, We suspect that the organic FM causes the non-wet... - Oct 28, 1999 by
Chris: Thanks. SMTnet has a "Library." Buried deep withi... - Oct 29, 1999 by davef
Chris A lot of people have reported sudden, fab lot related... - Oct 29, 1999 by John Thorup
Hi John, Thanks to your reply, just one question is it po... - Nov 04, 1999 by
Chris: You can have more than "one question!!!" Anyhow, y... - Nov 05, 1999 by davef
chris