Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2969
Hi , In one particular component we observed , its leads ... - Mar 16, 2019 by Ameen
that is iron oxide, see if you can shorten reflow profile. ... - Mar 18, 2019 by bukas
Thanks Bukas, will check and update on the same. ... - Mar 18, 2019 by Ameen