Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 7121
Hi Team, Can anyone suggest me best stencil opening for CCG... - Jul 24, 2019 by Ameen
Your solder stencil design should follow all basic rules for... - Jul 24, 2019 by davef
thanks dave .. I have one more query on the same CCGA. W... - Jul 30, 2019 by Ameen
Your inputs are always valuable and help a lot. Thanks for t... - Jul 30, 2019 by Ameen
Attached is the image of lead lift in ccga ... - Jul 30, 2019 by Ameen
I'd be surprised if CCGA leads were getting bent or tilted d... - Jul 30, 2019 by davef
Ameen: Send me your email address by selecting the link unde... - Jul 30, 2019 by davef
Hi Dave, lead is 80Pb/20Sn. Top joint off CCGA lead is SN6... - Jul 31, 2019 by Ameen
I don't get it. The liquidus of 80Pb/20Sn is like 280*C. You... - Aug 02, 2019 by davef
Hi Dave, Yes the lead was there before reflow. After refl... - Aug 07, 2019 by Ameen
Did you check the pin location accuracy before placement? I ... - Aug 09, 2019 by sssamw
Hi , Thanks for the reply. Yes CCGA was checked before pl... - Aug 13, 2019 by Ameen
And what is the solder paste selection recommendation for th... - Aug 21, 2019 by Ameen
From the picture you present, it is a pin in paste part with... - Aug 22, 2019 by sssamw
Hi , Its CCGA part . with normal PCB pad opening similar t... - Aug 23, 2019 by Ameen
Hi Everyone, Reducing the top heaters around 10 deg each at... - Dec 11, 2019 by Ameen