Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 7398
Ok, Question for all of you quality inspectors out there. ...
- Nov 21, 2019
by
scotceltic
Do you mean the void over the vias? That's normal phenomenon...
- Nov 21, 2019
by
sssamw
I'm worried about the voids that you have on the heel fillet...
- Nov 22, 2019
by
DWL
Thank you for the response. Nothing in the datasheet referr...
- Nov 26, 2019
by
scotceltic
I am more worried about those voids also instead of the void...
- Nov 26, 2019
by
scotceltic
It's hard to tell from the image but it looks like there isn...
- Nov 26, 2019
by
Steve Thomas
OK, if has concern on void in the function pin area, you nee...
- Nov 27, 2019
by
sssamw
The short answer is people are still arguing about what the ...
- Dec 10, 2019
by
SMTA-Norah
SMTA
Hi,
Below may help you out.
per IPC 7093 ( Design and ass...
- Dec 11, 2019
by
Ameen
Although this is not technically a bottom termination compon...
- Dec 11, 2019
by
Clockwatcher
Thank you all for the comments. They have been helpful to r...
- Dec 11, 2019
by
scotceltic
I agree with you in this case. The voids on ground pad of IC...
- Dec 20, 2019
by
GC_2019
Steve Thomas pointed the right question. Go and verify the d...
- Dec 30, 2019
by
Evtimov
I do faced this problem and and not solve. Fortunately, did ...
- Jan 04, 2020
by
SMTA-Davandran
SMTA