Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3599
Our Production facility wants to convert to Lead Free (SMT)....
- Dec 05, 2019
by
SMTA-June
SMTA
Not going be accused of rushing into things, eh?
Tons of st...
- Dec 06, 2019
by
davef
To me, the BIGGEST issue is <BR>
> process and ...
- Dec 06, 2019
by
kyleh04
I don't know, I just find process qualification a lot of pap...
- Dec 08, 2019
by
davef
Thank you!
...
- Dec 10, 2019
by
SMTA-June
SMTA
The one thing I haven't seen mentioned yet is developing the...
- Dec 11, 2019
by
Steve Thomas
From what I understand when ROHS was first implemented the E...
- Dec 11, 2019
by
Stephen
"A microscopic amount of lead on an 0402 joint makes th...
- Dec 11, 2019
by
Steve Thomas
Lead Free SMT
1. Stencil printer Squeegees s -should have Pb...
- Dec 26, 2019
by
Evtimov
&gt; Our Production facility wants to convert to Lea...
- Jan 06, 2020
by
Wellman Rau
It is not all of the product.
It is per separable homogeneou...
- Jan 06, 2020
by
Stephen