Hello, We are having problems with SMD wave soldering (ERS... - Dec 27, 2019 by anteiv
I could not see pictures of your board - please attach one o... - Dec 27, 2019 by Evtimov
As has already been mentioned, black residue is usually eith... - Dec 27, 2019 by Steve Thomas
In your video, it looks to me as though the bottom of the gl... - Dec 27, 2019 by robgd3
thank you for reply here is picture of the board https://i... - Dec 27, 2019 by anteiv
Using no-clean flux will make the boards very difficult to c... - Dec 27, 2019 by robgd3
Thanks Rob, this is excelent ... - Dec 30, 2019 by Evtimov
It looks like solder dross there or flux residue that not ac... - Dec 31, 2019 by sssamw
The video showing wave contact is not consistent and not sta... - Dec 31, 2019 by sssamw
thanks again for reply, we have now configured speed of tra... - Dec 31, 2019 by anteiv
We made much better contact of wave with board. There was no... - Jan 18, 2020 by anteiv