Hi,
I need help on how to address the solder wicking on the ...
- Jan 13, 2020
by
Avillaro2020
Hi Arnel,
I've used these before but with a 0.005" ste...
- Jan 14, 2020
by
Robl
I've worked with these quite a bit in the past as well. As ...
- Jan 14, 2020
by
dontfeedphils
Thanks Robl. I’ve contacted samtec followed their advice but...
- Jan 14, 2020
by
Avillaro2020
Hi Phil, thanks. I am successful using the same connector on...
- Jan 14, 2020
by
Avillaro2020
Avillaro,
would you say that vapor phase process was select...
- Jan 14, 2020
by
Evtimov
Hi Evtimov,
Thanks for your response.
Yes, the vapour phase ...
- Jan 14, 2020
by
Avillaro2020
Having 10c thermal differential is a lot. Trying different p...
- Jan 15, 2020
by
Evtimov
Hi Evtimov,
Thanks again!
The solder wicking/open solder jo...
- Jan 15, 2020
by
Avillaro2020
As far as the large thermal gradient I have on my thick and ...
- Jan 15, 2020
by
Avillaro2020
Avillaro,
I don't have hands on experience with Vapor Phase ...
- Jan 15, 2020
by
Evtimov