Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2277
Hi everyone I have problems welding QFN components in a 10-z... - Feb 11, 2020 by Sebas
Values and range definitions on your profile attachment are ... - Feb 11, 2020 by Evtimov
We had this problem at my old job. My understanding (from go... - Feb 11, 2020 by RobD
I was going to say, technically it's BTC, so I don't believe... - Feb 11, 2020 by dontfeedphils
hello Evtimov Thanks for your answer. I will analyze the cur... - Feb 11, 2020 by Sebas
Sebas, on your profile you have listed U2, U101, U102 and I... - Feb 11, 2020 by Evtimov
Yep....I just looked at a copy of IPC-610-G and am not 100% ... - Feb 11, 2020 by Steve Thomas
Hi Steve Thomas Effectively by IPC-610 standard specifies i... - Feb 11, 2020 by Sebas
Evtimov The areas analyzed are a standard oven curve accord... - Feb 11, 2020 by Sebas
Sebas, I suspect that your finding of needing the fillet fo... - Feb 11, 2020 by robgd3
Your profile should be close to this. ... - Feb 11, 2020 by Evtimov
hello robgd3 Thank you for your contribution based on your e... - Feb 11, 2020 by Sebas
Evtimov thank you very much for sharing this profile, we wil... - Feb 11, 2020 by Sebas
There are several areas you can check. Your profile is very ... - Feb 12, 2020 by SMTA-Alex SMTA
Evtimov SMTA-Alex Hi After the comments, we have analyzed ... - Feb 18, 2020 by Sebas
Sebas, some things in your profile don't make sense. 3 of yo... - Feb 18, 2020 by SMTA-Alex SMTA
Sebas, Curve you attached is using different temp table. We... - Feb 19, 2020 by Evtimov
Hello, The oven profil is not the solution! The only soluti... - Feb 20, 2020 by ben
Yes, this is for tin-lead profile. And for the QFN pins whic... - Feb 23, 2020 by sssamw