I would like to know when to consider top preheaters in a wa...
- Feb 19, 2020
by
toki
Use them always - they help for even preheat of the board. I...
- Feb 19, 2020
by
Evtimov
I would always have top and bottom preheaters in a solderwav...
- Feb 21, 2020
by
bruce
I used to work for an OEM that made professional audio equip...
- Feb 21, 2020
by
Steve Thomas
Thanks to all for the feedback, i will be going for top and ...
- Feb 21, 2020
by
toki