I am desperate. I have an 80S15 with a single line controlle... - Mar 05, 2020 by Katrina
My advice for what it is worth. Your description of the pro... - Mar 05, 2020 by sarason
I used to work with S15/F3, was a 10 years ago. 1. Test you... - Mar 09, 2020 by Kristof_K
Hello Kristof, We use 1 PC which does line control and progr... - Mar 09, 2020 by Katrina
Sadly, without line controller software you won't be able to... - Mar 09, 2020 by Kristof_K
Hello Sarason, Unfortunately the machine is no longer suppor... - Mar 09, 2020 by Katrina
We have the software and our PC has been running the machine... - Mar 09, 2020 by Katrina
Here is a few pictures. IMG_20200311_151400 shows the screen... - Mar 11, 2020 by Katrina
Katrina, it is one of both: 1. Communication error - try t... - Mar 16, 2020 by Evtimov
Thank you for your reply. So the machine should preform a ze... - Mar 16, 2020 by Katrina
You should be able to operate/troubleshoot machine on its ow... - Mar 17, 2020 by Evtimov
With LC off, the machine when told "Without LC" wi... - Mar 17, 2020 by Katrina
Katrina, if the machine will zero on its own, there is noth... - Mar 18, 2020 by Evtimov
I have replaced both cards on the machine and the card in th... - Mar 18, 2020 by Katrina