We are using Superior 515 flux to clean and tin selective so...
- Apr 01, 2020
by
ProcEng1
The brush also turned yellow.
...
- Apr 01, 2020
by
ProcEng1
Very interesting.Safety datasheet suggest acid that might tu...
- Apr 01, 2020
by
Evtimov
We did not try using water. Once the nozzles were left in t...
- Apr 01, 2020
by
ProcEng1
And this is why you see it only in Leaded process I guess.
...
- Apr 01, 2020
by
Evtimov
If you can find some, you might want to give Adipic Acid a t...
- Apr 02, 2020
by
Stephen