Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4278
Hi, We are currently using WonderMask PX Peelable Solder M... - Apr 22, 2020 by MVARGAS
We prefered kapton tape to peelable mask, though, there is a... - Apr 22, 2020 by robgd3
We use Wondermask 2211 and we haven't had issues with the ma... - Apr 22, 2020 by SMTA-Samy SMTA
Hi, thank you both for answering. Unfortunately, due to volu... - Apr 23, 2020 by MVARGAS
Is your board spending 40s on a molten solder at 500F? ... - Apr 27, 2020 by Evtimov
That's correct. This is because the component (switch) needs... - Apr 27, 2020 by MVARGAS
Are you watching for copper dissolution? At one place I was ... - Apr 28, 2020 by Stephen
PCB Electronics Ltd, a leading corporation focusing on one-s... - Apr 29, 2020 by Tomzhao2