Views: 821
I often need to wind a coil for transformers, solenoids, or ...
- Jul 24, 2020
by
jordanabshire
Look on the net for Paxolin or SRBP P1
...
- Jul 29, 2020
by
PhilC
You're asking about unclad FR4 [G10 is not flame retardant] ...
- Jul 29, 2020
by
davef