Hello,

We have recently bought ZipaTec select 250, we are having problems with offsets.

Somehow the offset of fluxer, wave and preheat dont match one another or the program we create.

The previous owners are of no help.

The main question i have is, does anyone have default offsets for the SELECT 250, or perhaps if someone is using it he can type in his own.

Or any advice regarding the problem at hand?

Thank you, Aljaž