I am wondering, I have an application for assembling a 0.4mm... - Mar 16, 2021 by Graham
I would recommend flux approach. I have placed tons of these... - Mar 17, 2021 by Evtimov
Hello Evtimov, thank you for your reply. I agree with you, u... - Mar 17, 2021 by Graham